journal article·2013-01-08

Li–O2 Battery Degradation by Lithium Peroxide (Li2O2): A Model Study

Reza Younesi, Maria Hahlin, Fredrik Björefors, Patrik Johansson, Kristina Edström

Chemistry of Materials· Volume 25· Issue 1
Publisher page

Abstract

The chemical stability of the Li–O 2 battery components (cathode and electrolyte) in contact with lithium peroxide (Li 2 O 2 ) was investigated using X-ray photoelectron spectroscopy (XPS). XPS is a versatile method to detect amorphous as well as crystalline decomposition products of both salts and solvents. Two strategies were employed. First, cathodes including carbon, α-MnO 2 catalyst, and Kynar binder (PVdF-HFP) were exposed to Li 2 O 2 and LiClO 4 in propylene carbonate (PC) or tetraethylene glycol dimethyl ether (TEGDME) electrolytes. The results indicated that Li 2 O 2 degrades TEGDME to carboxylate containing species and that the decomposition products, in turn, degraded the Kynar binder. The α-MnO 2 catalyst was unaffected. Second, Li 2 O 2 model surfaces were kept in contact with different electrolytes to investigate the chemical stability and also the resulting surface layer on Li 2 O 2 . Further, the XPS experiments revealed that the Li salts such as LiPF 6, LiBF 4, and LiClO 4 decomposed to form LiF or LiCl together with P–O or B–O bond containing compounds when exposed to Li 2 O 2 . PC decomposed to carbonate and ether based species. The degradation of the electrolytes increased from short to long exposure time indicating that the surface layer on Li 2 O 2 became thicker by increasing time. Overall, it was shown that a mixture of ethylene carbonate and diethyl carbonate (EC/DEC) is more robust in contact with Li 2 O 2 compared to PC.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advancements in Battery Materials · Advanced Battery Materials and Technologies · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Chemistry-Ångström Laboratory, Uppsala University, Box 538, SE-75121 Uppsala, Sweden

Department of Applied Physics, Chalmers University of Technology, SE-41296 Göteborg, Sweden

Alistore, European Research Institute, 33 Rue Saint-Leu, 80039 Amiens Cedex, France

References (43)

Show source-provided references
1. Christensen J. · J. Electrochem. Soc. · 2012 · 159 · R110.1149/2.086202jes ↗
2. Kraytsberg A. · J. Power Sources · 2011 · 196 · 88610.1016/j.jpowsour.2010.09.031 ↗
3. Bruce P. G. · Nat. Mater. · 2011 · 11 · 1910.1038/nmat3191 ↗
4. Cheng F. · Chem. Soc. Rev. · 2012 · 41 · 217210.1039/c1cs15228a ↗
5. Wang Y. · Chem. Com. · 2010 · 46 · 630510.1039/c0cc00074d ↗
6. Mizuno F. · Electrochemistry · 2010 · 78 · 40310.5796/electrochemistry.78.403 ↗
7. Freunberger S. A. · J. Am. Chem. Soc. · 2011 · 133 · 804010.1021/ja2021747 ↗
8. Xu W. · J. Power Sources · 2011 · 196 · 963110.1016/j.jpowsour.2011.06.099 ↗
9. Younesi R. · J. Phys. Chem. C · 2012 · 116 · 2067310.1021/jp302168h ↗
10. McCloskey B. D. · J. Phys. Chem. Lett. · 2011 · 2 · 116110.1021/jz200352v ↗
11. Freunberger S. A. · Angew. Chem., Int. Ed. · 2011 · 50 · 860910.1002/anie.201102357 ↗
12. Wang H. · Electrochim. Acta · 2012 · 64 · 2910.1016/j.electacta.2011.12.080 ↗
13. Younesi R. · J. Phys. Chem. C · 2012 · 116 · 1859710.1021/jp303691m ↗
14. Hyoung Oh, S. · Electrochem. Solid-State Lett. · 2011 · 14 · A18510.1149/2.003112esl ↗
15. Veith G. M. · J. Phys. Chem. Lett. · 2012 · 3 · 124210.1021/jz300430s ↗
16. Hong J. · Chem. Mater. · 2012 · 24 · 269210.1021/cm3005634 ↗
17. Younesi R. · J. Power Sources · 2013 · 225 · 4010.1016/j.jpowsour.2012.10.011 ↗
18. Laino T. · Chem.—Eur. J. · 2012 · 18 · 351010.1002/chem.201103057 ↗
19. McCloskey B. D. · J. Phys. Chem. Lett. · 2012 · 3 · 99710.1021/jz300243r ↗
20. Oswald S. · Anal. Bioanal. Chem. · 2011 · 400 · 69110.1007/s00216-010-4646-z ↗
21. Chalasani D. · ECS Electrochem. Lett. · 2012 · 1 · A3810.1149/2.010202eel ↗
22. Abraham K. M. · J. Electrochem. Soc. · 1996 · 143 · 110.1149/1.1836378 ↗
23. Zhang Z. · J. Phys. Chem. C · 2011 · 115 · 2553510.1021/jp2087412 ↗
24. Mitchell R. R. · Energy Environ. Sci. · 2011 · 4 · 295210.1039/c1ee01496j ↗
25. Peng Z. · Science · 2012 · 337 · 56310.1126/science.1223985 ↗
26. Cota L. G. · Acta Cryst. Sec. B · 2005 · 61 · 13310.1107/S0108768105003629 ↗
27. Wu H. · Philos. Mag. · 2007 · 87 · 337310.1080/14786430701286239 ↗
28. Zheng J. P. · J. Electrochem. Soc. · 2008 · 155 · A43210.1149/1.2901961 ↗
29. Younesi S. R. · J. Power Sources · 2011 · 196 · 983510.1016/j.jpowsour.2011.07.062 ↗
30. Dedryvère R. · Chem. Mater. · 2004 · 16 · 105610.1021/cm0311269 ↗
31. Edstrom K. · Electrochim. Acta · 2004 · 50 · 39710.1016/j.electacta.2004.03.049 ↗
32. Andersson A. M. · J. Power Sources · 2003 · 119 · 52210.1016/S0378-7753(03)00277-5 ↗
33. Lu Y.-C. · Chem. Mater. · 2009 · 21 · 440810.1021/cm900862v ↗
34. Kanamura K. · Chem. Mater. · 1997 · 4756 · 179710.1021/cm970042v ↗
35. Wade L. G. · 2010
36. Clover A. M. · J. Am. Chem. Soc. · 1922 · 44 · 110710.1021/ja01426a024 ↗
37. Bryantsev V. S. · J. Phys. Chem. A · 2012 · 116 · 712810.1021/jp301537w ↗
38. Black R. · J. Am. Chem. Soc. · 2012 · 134 · 290210.1021/ja2111543 ↗
39. Andersson A. M. · Electrochim. Acta · 2002 · 47 · 188510.1016/S0013-4686(02)00044-0 ↗
40. Dedryvère R. · J. Phys. Chem. B · 2006 · 110 · 1298610.1021/jp061624f ↗
41. Seah M. P. · Surf. Interface Anal. · 2012 · 44 · 49710.1002/sia.4816 ↗
42. Sloop S. E. · Electrochem. Solid-State Lett. · 2001 · 4 · A4210.1149/1.1353158 ↗
43. Nazri G. · J. Electrochem. Soc. · 1985 · 132 · 205010.1149/1.2114288 ↗