Abstract

The present study evaluated the durability of bond strength between zirconia and 3 different resin cements. Thirty stabilized tetragonal zirconium-dioxide blocks were duplicated in dual-curing resin core build-up material specimens. Resin blocks were randomly luted to zirconium surfaces using 1) Clearfil Esthetic Cement (CLF), 2) RelyX Unicem Aplicap (RELX), or 3) Multilink Automix (MLA). After 24 h, half of the specimens from each of the 3 groups were loaded in tension until fracture (0.5 mm/min). The remaining half were tested after 6,000 thermal cycles (5 to 55°C). Data were analyzed using 2-way ANOVA and the Tukey test (α = 0.05). Fractographic analysis was performed using a stereomicroscope. Tensile bond strength values were significantly affected by the luting agent system employed and by thermal aging (P < 0.001). The highest tensile bond strength values in non-thermal-aged groups were observed for specimens from the RELX and CLF groups. In contrast, in the thermal-aged groups, the highest tensile bond strength values were for the MLA and RELX groups. Moreover, while thermocycling significantly affected bond strengths in the RELX and CLF groups, the mean strength of the MLA group did not significantly change after aging. There was little difference in the distribution of failure modes in any group.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Endodontics and Root Canal Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. 1. Denry I, Kelly JR (2008) State of the art of zirconia for dental applications. Dent Mater 24, 299-307.10.1016/j.dental.2007.05.007 ↗
2. 10.1002/jbm.82023010510.1002/jbm.820230105 ↗
3. 3. Luthardt RG, Sandkuhl O, Reitz B (1999) Zirconia-TZP and alumina – advanced technologies for the manufacturing of single crowns. Eur J Prosthodont Restor Dent 7, 113-119.
4. 10.1016/S0142-9612(98)00010-610.1016/S0142-9612(98)00010-6 ↗
5. 5. Ortorp A, Kihl ML, Carlsson GE (2009) A 3-year retrospective and clinical follow-up study of zirconia single crowns performed in a private practice. J Dent 37, 731-736.10.1016/j.jdent.2009.06.002 ↗
6. 10.1177/15440591020810071110.1177/154405910208100711 ↗
7. 10.1067/mpr.2003.5010.1067/mpr.2003.50 ↗
8. 8. Dérand P, Dérand T (2000) Bond strength of luting cements to zirconium oxide ceramics. Int J Prosthodont 13, 131-135.
9. 10.1016/j.biomaterials.2004.02.03610.1016/j.biomaterials.2004.02.036 ↗
10. 10. Casucci A, Osorio E, Osorio R, Monticelli F, Toledano M, Mazzitelli C, Ferrari M (2009) Influence of different surface treatments on surface zirconia frameworks. J Dent 37, 891-897.10.1016/j.jdent.2009.06.013 ↗
11. 10.1016/j.dental.2005.04.01610.1016/j.dental.2005.04.016 ↗
12. 10.1016/j.dental.2005.11.03510.1016/j.dental.2005.11.035 ↗
13. 10.1002/jbm.b.3042410.1002/jbm.b.30424 ↗
14. 10.2334/josnusd.51.62910.2334/josnusd.51.629 ↗
15. 15. Aboushelib MN, Matinlinna JP, Salameh Z, Ounsi H (2008) Innovations in bonding to zirconia-based materials: Part I. Dent Mater 24, 1268-1272.10.1016/j.dental.2008.02.010 ↗
16. 16. Wegner SM, Kern M (2000) Long-term resin bond strength to zirconia ceramic. J Adhes Dent 2, 139-147.
17. 10.1002/jbm.b.3090810.1002/jbm.b.30908 ↗
18. 18. Goracci C, Cury AH, Cantoro A, Papacchini F, Tay FR, Ferrari M (2006) Microtensile bond strength and interfacial properties of self-etching and self-adhesive resin cements used to lute composite onlays under different seating forces. J Adhes Dent 8, 327-335.
19. 10.1016/j.dental.2004.03.00210.1016/j.dental.2004.03.002 ↗
20. 10.1016/j.prosdent.2005.04.01110.1016/j.prosdent.2005.04.011 ↗
21. 10.1016/j.dental.2005.04.02110.1016/j.dental.2005.04.021 ↗
22. 22. Palacios RP, Johnson GH, Phillips KM, Raigrodski AJ (2006) Retention of zirconium oxide ceramic crowns with three types of cement. J Prosthet Dent 96, 104-114.10.1016/j.prosdent.2006.06.001 ↗
23. 10.1016/j.prosdent.2004.07.00110.1016/j.prosdent.2004.07.001 ↗
24. 24. Bottino MA, Valandro LF, Scotti R, Buso L (2005) Effect of surface treatments on the resin bond to zirconium-based ceramic. Int J Prosthodont 18, 60-65.10.1016/j.prosdent.2005.05.011 ↗
25. 25. Oyagüe RC, Monticelli F, Toledano M, Osorio E, Ferrari M, Osorio R (2009) Effect of water aging on microtensile bond strength of dual-cured resin cements to pre-treated sintered zirconium-oxide ceramics. Dent Mater 25, 392-399.10.1016/j.dental.2008.09.002 ↗
26. 10.1016/S0109-5641(98)00011-610.1016/S0109-5641(98)00011-6 ↗
27. 10.1016/j.dental.2005.11.04010.1016/j.dental.2005.11.040 ↗
28. 10.1016/j.prosdent.2004.12.00210.1016/j.prosdent.2004.12.002 ↗
29. 29. Bailey LF, Benett RJ (1988) DICOR surface treatments for enhanced bonding. J Dent Res 67, 925-931.10.1177/00220345880670060701 ↗
30. 30. Atta MO, Smith BGN, Brown D (1990) Bond strengths of three chemical adhesive cements adhered to a nickel chromium alloy for direct bonded retainers. J Prosthet Dent 63, 137-143.10.1016/0022-3913(90)90096-U ↗
31. 31. Chang JC, Powers JM, Hart D (1993) Bond strength of composite to alloy treated with bonding systems. J Prosthodont 2, 110-114.10.1111/j.1532-849X.1993.tb00391.x ↗
32. 10.1016/S0022-3913(05)80200-810.1016/S0022-3913(05)80200-8 ↗
33. 10.1016/j.dental.2003.10.01410.1016/j.dental.2003.10.014 ↗
34. 34. Braden M, Causton EE, Clarke RL (1976) Diffusion of water in composite filling materials. J Dent Res 55, 730-732.10.1177/00220345760550050501 ↗