Radiopacity of conventional, resin-modified glass ionomer, and resin-based luting materials
Source abstract
Abstract
The purpose of the present study was to evaluate the radiopacity of currently available dental luting materials. Five conventional cements, six resin-modified glass ionomers (RMGIs), two methyl methacrylate (MMA)-based acrylic resins (eight shades), and nine composite luting materials were evaluated. Radiographs of the specimens were taken together with tooth slices and aluminum step wedges. The density of the specimens was determined with a densitometer and was expressed in terms of the equivalent thickness of aluminum per 2.0-mm unit thickness of specimen. The radiopacity values for human enamel and dentin were 4.3 and 2.3 mm Al/2.0 mm specimen, respectively. The values for materials ranged from 5.1 to 12.9 for conventional luting materials, from 3.4 to 6.3 for RMGIs, from less than 0.5 to 7.3 for MMA resins, and from 2.3 to 9.9 for the composite luting materials. A zinc phosphate cement showed the highest value (12.9), whereas five shades of MMA resin resulted in the lowest value (less than 0.5). Two RMGIs and three composite luting materials exhibited radiopacity values between those of enamel (4.3) and dentin (2.3). It can be concluded that the radiopacity value of luting materials varies considerably, and that care must be taken when selecting luting materials, considering the material composition of restorations.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Radiography and Imaging · Endodontics and Root Canal Treatments
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. 1. Espelid I, Tveit AB, Erickson RL, Keck SC, Glasspoole EA (1991) Radiopacity of restorations and detection of secondary caries. Dent Mater 7, 114-117.10.1016/0109-5641(91)90056-5 ↗
2. 2. Prévost AP, Forest D, Tanguay R, DeGrandmont P (1990) Radiopacity of glass ionomer dental materials. Oral Surg Oral Med Oral Pathol 70, 231-235.10.1016/0030-4220(90)90125-C ↗
3. 3. Goshima T, Goshima Y (1991) Optimum radiopacity of composite inlay materials and cements. Oral Surg Oral Med Oral Pathol 72, 257-260.10.1016/0030-4220(91)90173-A ↗
4. 4. El-Mowafy OM, Benmergui C (1994) Radiopacity of resin-based inlay luting cements. Oper Dent 19, 11-15.
5. 5. International Organization for Standardization (2000) Dentistry – Polymer-based filling, restorative and luting materials. ISO 4049: 2000, Geneve.
6. 6. Williams JA, Billington RW (1990) The radiopacity of glass ionomer dental materials. J Oral Rehabil 17, 245-248.10.1111/j.1365-2842.1990.tb00005.x ↗
7. 7. Matsumura H, Sueyoshi M, Tanaka T, Atsuta M (1993) Radiopacity of dental cements. Am J Dent 6, 43-45.
8. 8. Skartveit L, Halse A (1996) Radiopacity of glass ionomer materials. J Oral Rehabil 23, 1-4.10.1111/j.1365-2842.1996.tb00803.x ↗
9. 9. Akerboom HB, Kreulen CM, van Amerongen WE, Mol A (1993) Radiopacity of posterior composite resins, composite resin luting cements, and glass ionomer lining cements. J Prosthet Dent 70, 351-355.10.1016/0022-3913(93)90221-9 ↗
10. 10. Attar N, Tam LE, McComb D (2003) Mechanical and physical properties of contemporary dental luting agents. J Prosthet Dent 89, 127-134.10.1067/mpr.2003.20 ↗
11. 11. Fonseca RB, Branco CA, Soares PV, Correr-Sobrinho L, Haiter-Neto F, Fernandes-Neto AJ, Soares CJ (2006) Radiodensity of base, liner and luting dental materials. Clin Oral Investig 10, 114-118.10.1007/s00784-005-0030-3 ↗
12. 12. Rasimick BJ, Gu S, Deutsch AS, Musikant BL (2007) Measuring the radiopacity of luting cements, dowels, and core build-up materials with a digital radiography system using a CCD sensor. J Prosthodont 16, 357-364.10.1111/j.1532-849X.2007.00209.x ↗
13. 13. Shah PM, Sidhu SK, Chong BS, Ford TR (1997) Radiopacity of resin-modified glass ionomer liners and bases. J Prosthet Dent 77, 239-242.10.1016/S0022-3913(97)70179-3 ↗