Plasma-Enhanced Atomic Layer Deposition of Silver Thin Films
Source abstract
Abstract
Thermal properties of various silver precursors known in the literature were evaluated in order to discover which precursor is the most suitable one for plasma-enhanced atomic layer deposition (PEALD) of silver thin films. Ag(fod)(PEt 3 ) (fod = 2,2-dimethyl-6,6,7,7,8,8,8-heptafluorooctane-3,5-dionato) was found to be the best choice. Using Ag(fod)(PEt 3 ) together with plasma-activated hydrogen, silver thin films were deposited at growth temperatures of 120–150 °C, and ALD-type saturative growth was achieved at 120–140 °C. At 120 °C, the growth rate was 0.03 nm per cycle. The plasma exposure time had also an effect on the growth rate: with shorter exposure times, the growth rate was lower over the whole deposition area. The films deposited at 120 °C contained relatively small amounts of impurities, but these still affected the electrical properties of the films. The resistivities were relatively low: about 20 nm thick films had a resistivity of 6–8 μΩ·cm. The morphology and the crystal structure of the films were analyzed as well.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Semiconductor materials and devices · Catalytic Processes in Materials Science · ZnO doping and properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Laboratory of Inorganic Chemistry, University of Helsinki, P.O. Box 55, FI-00014 University of Helsinki, Finland
Department of Physics, University of Jyväskylä, P.O. Box 35, FI-40014 University of Jyväskylä, Finland
References (30)
Show source-provided references
1. Ritala, M.; Niinistö, J.InChemical Vapour Deposition: Precursors, Processes and Applications;Royal Society of Chemistry:Cambridge, UK, 2008; pp158–206.
2. George S. M. · Chem. Rev. · 2010 · 110 · 11110.1021/cr900056b ↗
3. Ozbay E. · Science · 2006 · 311 · 18910.1126/science.1114849 ↗
4. Barnes W. L. · Nature · 2003 · 424 · 82410.1038/nature01937 ↗
5. International Technology Roadmap for Semiconductors. [Online] 2009; http://www.itrs.net/Links/2009ITRS/Home2009.htm.
6. Piedade A. P. · Nanotechnology · 2007 · 18 · 10510310.1088/0957-4484/18/10/105103 ↗
7. Im H. · ACS Nano · 2010 · 4 · 94710.1021/nn901842r ↗
8. De Vries J. W. C. · Thin Solid Films · 1988 · 167 · 2510.1016/0040-6090(88)90478-6 ↗
9. Liu H. · ACS Nano · 2010 · 4 · 313910.1021/nn100466p ↗
10. Kapaklis V. · Thin Solid Films · 2006 · 510 · 13810.1016/j.tsf.2005.12.311 ↗
11. Yuan Z. · Chem. Vap. Deposition · 1995 · 7 · 1696
12. Serghini-Monim S. · J. Phys. Chem. · 1995 · 99 · 923010.1021/j100022a041 ↗
13. Gao L. · Mater. Sci. Semicond. Process · 2004 · 7 · 33110.1016/j.mssp.2004.09.128 ↗
14. Gao L. · Microelectron. Eng. · 2005 · 82 · 29610.1016/j.mee.2005.07.078 ↗
15. Niskanen A. · Chem. Vap. Deposition · 2007 · 1 · 40810.1002/cvde.200606519 ↗
16. Chalker P. R. · Nanotechnology · 2010 · 21 · 40560210.1088/0957-4484/21/40/405602 ↗
17. Kottke T. · J. Appl. Crystallogr. · 1993 · 26 · 61510.1107/S0021889893002018 ↗
18. Sheldrick G. M. · 2000
19. Sheldrick G. M. · Acta Crystallogr., Sect. A. · 2008 · 64 · 11210.1107/S0108767307043930 ↗
20. 2000
21. Waldo R. A. · Microbeam Anal. · 1988 · 310
22. Putkonen M. · Anal. Bioanal. Chem. · 2005 · 382 · 179110.1007/s00216-005-3365-3 ↗
23. Szlyk E. · Dalton. Trans. · 2010 · 39 · 182310.1039/b911741e ↗
24. Edvards D. A. · J. Mater. Chem. · 2003 · 13 · 56310.1039/b210085c ↗
25. Zanotto L. · Chem. Vap. Deposition · 2004 · 10 · 20710.1002/cvde.200306290 ↗
26. Darr J. A. · Inorg. Chem. · 1998 · 37 · 549110.1021/ic971206c ↗
27. Fragalà E. M. · Chem. Mater. · 2000 · 12 · 29010.1021/cm9911215 ↗
28. Ngo S. C. · Polyhedron · 2002 · 21 · 128910.1016/S0277-5387(02)00980-4 ↗
29. Yuan Z. · J. Mater. Chem. · 1995 · 5 · 30310.1039/JM9950500303 ↗
30. Bahlawane N. · Chem. Vap. Deposition · 2007 · 13 · 40110.1002/cvde.200706610 ↗