Abstract

PURPOSE: The purpose of this study was to investigate the influence of inner crown thickness on the bonding strength of porcelain fused to Co-Cr alloy endocrown by shear strength test. METHODS: According to the molar average anatomical data to obtain a simplified model for endocrowns, porcelain fused to Co-Cr alloy endocrowns were fabricated with four inner crown thicknesses: 0.3 mm, 0.5 mm, 0.8 mm, and 1.0 mm group, eight specimens were fabricated for each thickness group. Shear bond strength test was used to observe the metal-porcelain bonding strength, scanning electron microscope (SEM) and energy dispersive spectrometer (EDS) analysis were performed after the test to evaluate the interface of metal-porcelain. RESULTS: The shear bond strength means (in MPa) were: 10.50 ± 2.55 (0.3 mm), 13.21 ± 2.27 (0.5 mm), 14.47 ± 1.46 (0.8 mm), and 15.78 ± 2.81 (1.0 mm), one-way ANOVA showed that there was a statistically significant difference among the thicknesses (P < 0.05). The SEM observation showed tight bonding, and the EDS analysis showed element diffusion phenomenon at the metal-porcelain interface. CONCLUSION: The bonding strength of porcelain fused to Co-Cr alloy endocrown varied according to the different thickness of inner crown and the thinner inner crown was recommended for tooth defects with limited prosthodontic space.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Endodontics and Root Canal Treatments

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Prosthodontics, Hainan Stomatological Hospital

References (25)

Show source-provided references
1. 1. Tzimas K, Tsiafitsa M, Gerasimou P, Tsitrou E (2018) Endocrown restorations for extensively damaged posterior teeth: clinical performance of three cases. Restor Dent Endod 43, e38.10.5395/rde.2018.43.e38 ↗
2. 2. Dogui H, Abdelmalek F, Amor A, Douki N (2018) Endocrown: an alternative approach for restoring endodontically treated molars with large coronal destruction. Case Rep Dent 2018, 1581952.10.1155/2018/1581952 ↗
3. 3. Govare N, Contrepois M (2020) Endocrowns: a systematic review. J Prosthet Dent 123, 411-418. e9.10.1016/j.prosdent.2019.04.009 ↗
4. 4. Sedrez-Porto JA, Münchow EA, Valente LL, Cenci MS, Pereira-Cenci T (2019) New material perspective for endocrown restorations: effects on mechanical performance and fracture behavior. Braz Oral Res 33, e012.10.1590/1807-3107bor-2019.vol33.0012 ↗
5. 5. Alhazzani SA, Aldossary MS (2019) Metal endocrown approach for a maxillary second molar: a novel technique. Gen Dent 67, 67-71.
6. 6. El Ghoul WA, Özcan M, Ounsi H, Tohme H, Salameh Z (2020) Effect of different CAD-CAM materials on the marginal and internal adaptation of endocrown restorations: an in vitro study. J Prosthet Dent 123, 128-134.10.1016/j.prosdent.2018.10.024 ↗
7. 7. Grimaudo NJ (2001) Biocompatibility of nickel and cobalt dental alloys. Gen Dent 49, 498-503.
8. 8. Al Jabbari YS (2014) Physico-mechanical properties and prosthodontic applications of Co-Cr dental alloys: a review of the literature. J Adv Prosthodont 6, 138-145.10.4047/jap.2014.6.2.138 ↗
9. 9. Anusavice KJ, Hojjatie B, Dehoff PH (1986) Influence of metal thickness on stress distribution in metal-ceramic crowns. J Dent Res 65, 1173-1178.10.1177/00220345860650091201 ↗
10. 10. Ekren O, Ozkomur A, Ucar Y (2018) Effect of layered manufacturing techniques, alloy powders, and layer thickness on metal-ceramic bond strength. J Prosthet Dent 119, 481-487.10.1016/j.prosdent.2017.04.007 ↗
11. 11. Kaleli N, Ural Ç, Özköylü G, Duran İ (2019) Effect of layer thickness on the marginal and internal adaptation of laser-sintered metal frameworks. J Prosthet Dent 121, 922-928.10.1016/j.prosdent.2018.08.018 ↗
12. 12. Diniz AC, Nascimento RM, Souza JC, Henriques BB, Carreiro AF (2014) Fracture and shear bond strength analyses of different dental veneering ceramics to zirconia. Mater Sci Eng C Mater Biol Appl 38, 79-84.10.1016/j.msec.2014.01.032 ↗
13. 13. Heintze SD, Rousson V (2010) Survival of zirconia- and metal-supported fixed dental prostheses: a systematic review. Int J Prosthodont 23, 493-502.
14. 14. Benetti P, Pelogia F, Valandro LF, Bottino MA, Bona AD (2011) The effect of porcelain thickness and surface liner application on the fracture behavior of a ceramic system. Dent Mater 27, 948-953.10.1016/j.dental.2011.05.009 ↗
15. 15. Henriques B, Soares D, Silva FS (2012) Microstructure, hardness, corrosion resistance and porcelain shear bond strength comparison between cast and hot pressed CoCrMo alloy for metal-ceramic dental restorations. J Mech Behav Biomed Mater 12, 83-92.10.1016/j.jmbbm.2012.03.015 ↗
16. 16. Toptan F, Alves AC, Henriques B, Souza JC, Coelho R, Silva FS et al. (2013) Influence of the processing route of porcelain/Ti-6Al-4V interfaces on shear bond strength. J Mech Behav Biomed Mater 20, 327-337.10.1016/j.jmbbm.2013.02.003 ↗
17. 17. Lima JM, Souza AC, Anami LC, Bottino MA, Melo RM, Souza RO (2013) Effects of thickness, processing technique, and cooling rate protocol on the flexural strength of a bilayer ceramic system. Dent Mater 29, 1063-1072.10.1016/j.dental.2013.07.019 ↗
18. 18. Ereifej N, Rodrigues FP, Silikas N, Watts DC (2011) Experimental and FE shear-bonding strength at core/veneer interfaces in bilayered ceramics. Dent Mater 27, 590-597.10.1016/j.dental.2011.03.001 ↗
19. 19. Fernandes Neto AJ, Panzeri H, Neves FD, Prado RA, Mendonça G (2006) Bond strength of three dental porcelains to Ni-Cr and Co-Cr-Ti alloys. Braz Dent J 17, 24-28.10.1590/S0103-64402006000100006 ↗
20. 20. Abi-Rached Fde O, Fonseca RG, Haneda IG, de Almeida-Júnior AA, Adabo GL (2012) The effect of different surface treatments on the shear bond strength of luting cements to titanium. J Prosthet Dent 108, 370-376.10.1016/S0022-3913(12)60194-2 ↗
21. 21. Henriques B, Soares D, Silva FS (2011) Shear bond strength of a hot pressed Au-Pd-Pt alloy-porcelain dental composite. J Mech Behav Biomed Mater 4, 1718-1726.10.1016/j.jmbbm.2011.05.029 ↗
22. 22. Serra-Prat J, Cano-Batalla J, Cabratosa-Termes J, Figueras-Àlvarez O (2014) Adhesion of dental Porcelain to cast, milled, and laser-sintered cobalt-chro-mium alloys: shear bond strength and sensitivity to thermocycling. J Prosthet Dent 112, 600-605.10.1016/j.prosdent.2014.01.004 ↗
23. 23. Vásquez VZ, Ozcan M, Kimpara ET (2009) Evaluation of interface characterization and adhesion of glass ceramics to commercially pure titanium and gold alloy after thermal- and mechanical-loading. Dent Mater 25, 221-231.10.1016/j.dental.2008.07.002 ↗
24. 24. Henriques B, Gasik M, Soares D, Silva FS (2012) Experimental evaluation of the bond strength between a CoCrMo dental alloy and porcelain through a composite metal-ceramic graded transition interlayer. J Mech Behav Biomed Mater 13, 206-214.10.1016/j.jmbbm.2012.04.019 ↗
25. 25. Swain MV (2009) Unstable cracking (chipping) of veneering porcelain on all-ceramic dental crowns and fixed partial dentures. Acta Biomater 5, 1668-1677.10.1016/j.actbio.2008.12.016 ↗