journal article·2019Open access

Fracture resistance of monolithic and veneered all-ceramic four-unit posterior fixed dental prostheses after artificial aging

Merve B. Güngör, Seçil K. Nemli, Bilge T. Bal, Evşen Tamam, Handan Yılmaz, Cemal Aydın

Journal of Oral Science· Volume 61· Issue 2

Abstract

This study compared the fracture resistance of monolithic and veneered all-ceramic four-unit posterior fixed dental prostheses (FDPs) generated by computer-aided design/computer-aided manufacturing (CAD/CAM) after aging in a mastication simulator. Four-unit FDPs were designed from six different all-ceramic systems: 1) monolithic lithium disilicate (M-E), 2) monolithic zirconia (M-TZI), 3) veneered zirconia by conventional layering (V-L), 4) veneered zirconia by lithium disilicate pressing (V-P), 5) veneered zirconia by lithium disilicate fusing (CAD-F-E), and 6) veneered zirconia by feldspathic ceramic cementing (CAD-C-CB). The specimens were divided into control and aging groups (n = 10 per group). The aging process included both thermocycling and mechanical loading and was followed by fracture resistance testing. All specimens in the M-E, M-TZI, and V-L groups survived; however, all specimens in the V-P group were fractured during artificial aging. The highest fracture resistance values were observed in the M-TZI group. According to the fracture resistance test, connector fractures were the most frequent type of failure. M-TZI and M-E FDPs revealed no failures during aging and showed higher fracture resistance than the veneered groups. Among the veneered zirconia framework groups, V-L FDPs showed the highest success rate during aging, while the fracture resistance was similar among all the veneered zirconia groups.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Dental Research and COVID-19

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Prosthodontics, Faculty of Dentistry, Gazi University

References (44)

Show source-provided references
1. 1. Pjetursson BE, Lang NP (2008) Prosthetic treatment planning on the basis of scientific evidence. J Oral Rehabil 35, 72-79.10.1111/j.1365-2842.2007.01824.x ↗
2. 2. Baldassarri M, Zhang Y, Thompson VP, Rekow ED, Stappert CF (2011) Reliability and failure modes of implant-supported zirconium-oxide fixed dental prostheses related to veneering techniques. J Dent 39, 489-498.10.1016/j.jdent.2011.04.006 ↗
3. 3. Chaar M, Witkowski S, Strub J, Att W (2013) Effect of veneering technique on the fracture resistance of zirconia fixed dental prostheses. J Oral Rehabil 40, 51-59.10.1111/j.1365-2842.2012.02323.x ↗
4. 4. Alghazzawi TF (2016) Advancements in CAD/CAM technology: options for practical implementation. J Prosthodont Res 60, 72-84.10.1016/j.jpor.2016.01.003 ↗
5. 5. Piconi C, Maccauro G (1999) Zirconia as a ceramic biomaterial. Biomaterials 20, 1-25.10.1016/S0142-9612(98)00010-6 ↗
6. 6. Tinschert J, Natt G, Mautsch W, Augthun M, Spiekermann H (2001) Fracture resistance of lithium disilicate, alumina, and zirconia-based three-unit fixed partial dentures: a laboratory study. Int J Prosthodont 14, 231-238.
7. 7. Raigrodski AJ, Hillstead MB, Meng GK, Chung KH (2012) Survival and complications of zirconia-based fixed dental prostheses: a systematic review. J Prosthet Dent 107, 170-177.10.1016/S0022-3913(12)60051-1 ↗
8. 8. Schmitter M, Mueller D, Rues S (2013) In vitro chipping behaviour of all-ceramic crowns with a zirconia framework and feldspathic veneering: comparison of CAD/CAM-produced veneer with manually layered veneer. J Oral Rehabil 40, 519-525.10.1111/joor.12061 ↗
9. 9. Roumanas ED (2013) The clinical reliability of zirconia-based fixed dental prostheses appears acceptable but further research is necessary. J Evid Based Dent Pract 13, 14-15.10.1016/j.jebdp.2012.12.004 ↗
10. 10. Naenni N, Bindl A, Sax C, Hämmerle C, Sailer I (2015) A randomized controlled clinical trial of 3-unit posterior zirconia-ceramic fixed dental prostheses (FDP) with layered or pressed veneering ceramics: 3-year results. J Dent 43, 1365-1370.10.1016/j.jdent.2015.07.013 ↗
11. 11. Beuer F, Schweiger J, Eichberger M, Kappert HF, Gernet W, Edelhoff D (2009) High-strength CAD/CAM-fabricated veneering material sintered to zirconia copings a new fabrication mode for all-ceramic restorations. Dent Mater 25, 121-128.10.1016/j.dental.2008.04.019 ↗
12. 13. Lameira DP, De Souza GM (2015) Fracture strength of aged monolithic and bilayer zirconia-based crowns. Biomed Res Int 2015, 418641.
13. 14. Basso G, Moraes R, Borba M, Duan Y, Griggs JA, Della Bona A (2016) Reliability and failure behavior of CAD-on fixed partial dentures. Dent Mater 32, 624-630.10.1016/j.dental.2016.01.013 ↗
14. 15. Sulaiman TA, Abdulmajeed AA, Donovan TE, Cooper LF, Walter R (2016) Fracture rate of monolithic zirconia restorations up to 5 years: a dental laboratory survey. J Prosthet Dent 116, 436-439.10.1016/j.prosdent.2016.01.033 ↗
15. 16. Schultheis S, Strub JR, Gerds TA, Guess PC (2013) Monolithic and bi-layer CAD/CAM lithium-disilicate versus metal-ceramic fixed dental prostheses: comparison of fracture loads and failure modes after fatigue. Clin Oral Invest 17, 1407-1413.10.1007/s00784-012-0830-1 ↗
16. 17. Johansson C, Kmet G, Rivera J, Larsson C, Vult Von Steyern P (2014) Fracture strength of monolithic all-ceramic crowns made of high translucent yttrium oxide-stabilized zirconium dioxide compared to porcelain-veneered crowns and lithium disilicate crowns. Acta Odontol Scand 72, 145-153.10.3109/00016357.2013.822098 ↗
17. 18. Valenti M, Valenti A (2009) Retrospective survival analysis of 261 lithium disilicate crowns in a private general practice. Quintessence Int 40, 573-579.
18. 19. Zhao K, Wei Y-R, Pan Y, Zhang XP, Swain MV, Guess PC (2014) Influence of veneer and cyclic loading on failure behavior of lithium disilicate glass-ceramic molar crowns. Dent Mater 30, 164-171.10.1016/j.dental.2013.11.001 ↗
19. 20. Nawafleh N, Hatamleh M, Elshiyab S, Mack F (2016) Lithium disilicate restorations fatigue testing parameters: a systematic review. J Prosthodont 25, 116-126.10.1111/jopr.12376 ↗
20. 21. Beuer F, Stimmelmayr M, Gueth JF, Edelhoff D, Naumann M (2012) In vitro performance of full-contour zirconia single crowns. Dent Mater 28, 449-456.10.1016/j.dental.2011.11.024 ↗
21. 22. Nordahl N, von Steyern PV, Larsson C (2015) Fracture strength of ceramic monolithic crown systems of different thickness. J Oral Sci 57, 255-261.10.2334/josnusd.57.255 ↗
22. 23. Güngör MB, Nemli SK (2018) Fracture resistance of CAD-CAM monolithic ceramic and veneered zirconia molar crowns after aging in a mastication simulator. J Prosthet Dent, 119, 473-480.10.1016/j.prosdent.2017.05.003 ↗
23. 24. Ambré MJ, Aschan F, von Steyern PV (2013) Fracture strength of yttria-stabilized zirconium-dioxide (Y-TZP) fixed dental prostheses (FDPS) with different abutment core thicknesses and connector dimensions. J Prosthodont 22, 377-382.10.1111/jopr.12003 ↗
24. 25. Lüthy H, Filser F, Loeffel O, Schumacher M, Gauckler LJ, Hammerle CH (2005) Strength and reliability of four-unit all-ceramic posterior bridges. Dent Mater 21, 930-937.10.1016/j.dental.2004.11.012 ↗
25. 26. Kohorst P, Herzog TJ, Borchers L, Stiesch-Scholz M (2007) Load-bearing capacity of all-ceramic posterior four-unit fixed partial dentures with different zirconia frameworks. Eur J Oral Sci 115, 161-166.10.1111/j.1600-0722.2007.00429.x ↗
26. 27. Larsson C, Holm L, Lövgren N, Kokubo Y, Vult von Steyern P (2007) Fracture strength of four-unit Y-TZP FPD cores designed with varying connector diameter. An in-vitro study. J Oral Rehabil 34, 702-709.10.1111/j.1365-2842.2007.01770.x ↗
27. 28. Kelly JR (2006) Evidence-based decision making: guide to reading the dental materials literature. J Prosthet Dent 95,152-160.10.1016/j.prosdent.2005.10.016 ↗
28. 29. Rosentritt M, Behr M, Gebhard R, Handel G (2006) Influence of stress simulation parameters on the fracture strength of all-ceramic fixed-partial dentures. Dent Mater 22, 176-182.10.1016/j.dental.2005.04.024 ↗
29. 30. Studart AR, Filser F, Kocher P, Gauckler LJ (2017) Fatigue of zirconia under cyclic loading in water and its implications for the design of dental bridges. Dent Mater 23, 106-114.10.1016/j.dental.2005.12.008 ↗
30. 31. Özcan M, Jonasch M (2018) Effect of cyclic fatigue tests on aging and their translational implications for survival of all-ceramic tooth-borne single crowns and fixed dental prostheses. J Prosthodont, 27, 364-375.10.1111/jopr.12566 ↗
31. 32. Fontijn-Tekamp F, Slagter A, Van Der Bilt A, Van ‘T Hof MA, Witter DJ, Kalk W et al. (2000) Biting and chewing in overdentures, full dentures, and natural dentitions. J Dent Res 79, 1519-1524.10.1177/00220345000790071501 ↗
32. 33. Morneburg TR, Pröschel PA (2002) Measurement of masticatory forces and implant loads: a methodologic clinical study. Int J Prosthodont 15, 20-27.
33. 34. Bömicke W, Rues S, Hlavacek V, Rammelsberg P, Schmitter M (2016) Fracture behavior of minimally invasive, posterior, and fixed dental prostheses manufactured from monolithic zirconia. J Esthet Restor Dent 28, 367-381.10.1111/jerd.12242 ↗
34. 35. Mahmood DJH, Linderoth EH, Wennerberg A, Vult Von Steyern P (2016) Influence of core design, production technique, and material selection on fracture behavior of yttria-stabilized tetragonal zirconia polycrystal fixed dental prostheses produced using different multilayer techniques: split-file, over-pressing, and manually built-up veneers. Clin Cosmet Invest Dent 8, 15-27.10.2147/CCIDE.S94343 ↗
35. 36. Rosentritt M, Behr M, Scharnagl P, Handel G, Kolbeck C (2011) Influence of resilient support of abutment teeth on fracture resistance of all-ceramic fixed partial dentures: an in vitro study. Int J Prosthodont 24, 465-468.
36. 37. Ereifej N, Silikas N, Watts DC (2008) Initial versus final fracture of metal-free crowns, analyzed via acoustic emission. Dent Mater 24, 1289-1295.10.1016/j.dental.2008.04.010 ↗
37. 38. Fischer J, Stawarczyk B, Trottmann A, Hämmerle CH (2009) Impact of thermal properties of veneering ceramics on the fracture load of layered Ce-TZP/A nanocomposite frameworks. Dent Mater 25, 326-330.10.1016/j.dental.2008.08.001 ↗
38. 39. Sundh A, Molin M, Sjögren G (2005) Fracture resistance of yttrium oxide partially-stabilized zirconia all-ceramic bridges after veneering and mechanical fatigue testing. Dent Mater 21, 476-482.10.1016/j.dental.2004.07.013 ↗
39. 40. Aboushelib MN, de Kler M, van der Zel JM, Feilzer AJ (2008) Effect of veneering method on the fracture and bond strength of bilayered zirconia restorations. Int J Prosthodont 21, 237-240.
40. 41. Amaral M, Villefort RF, Melo RM, Pereira GKR, Zhang Y, Valandro LF et al. (2017) Fatigue limit of monolithic Y-TZP three-unit-fixed dental prostheses: effect of grinding at the gingival zone of the connector. J Mech Behav Biomed Mater 72, 159-162.10.1016/j.jmbbm.2017.03.002 ↗
41. 42. Limmer B, Sanders AE, Reside G, Cooper LF (2014) Complications and patient-centered outcomes with an implant-supported monolithic zirconia fixed dental prosthesis: 1 year results. J Prosthodont 23, 267-275.10.1111/jopr.12110 ↗
42. 43. Belli R, Petschelt A, Hofner B, Hajto J, Scherrer SS, Lohbauer U (2016) Fracture rates and lifetime estimations of CAD/CAM all-ceramic restorations. J Dent Res 95, 67-73.10.1177/0022034515608187 ↗
43. 44. Kamio S, Komine F, Taguchi K, Iwasaki T, Blatz MB, Matsumura H (2015) Effects of framework design and layering material on fracture strength of implant-supported zirconia-based molar crowns. Clin Oral Implants Res 26, 1407-1413.10.1111/clr.12468 ↗
44. 45. Att W, Grigoriadou M, Strub J (2007) ZrO2 three-unit fixed partial dentures: comparison of failure load before and after exposure to a mastication simulator. J Oral Rehabil 34, 282-290.10.1111/j.1365-2842.2006.01705.x ↗